Titanium gypsum bụ ụdị ihe mkpofu nwere dihydrate gypsum dị ka ihe bụ isi, nke a na-emepụta site na itinye lime (ma ọ bụ calcium carbonate) iji mee ka nnukwu mmiri mkpofu acid ghara ịdị irè iji gwọọ mmiri mkpofu acid mgbe a na-emepụta titanium dioxide site na usoro sulfuric acid. Mwepụ nke titanium gypsum abụghị naanị na ọ na-ewe ọtụtụ ala ma na-emerụ gburugburu ebe obibi, kamakwa ọ na-ebute nnukwu ibu arọ akụ na ụba nye ụlọ ọrụ titanium dioxide. Enwere ike iji titanium gypsum mee ihe na-egbochi simenti mgbe ejiri igwe egweri ya. Guilin Hongcheng bụ ọkachamara na-emepụtatitaniumigwe igwe gypsum.Ihe ndị a na-akọwa otu esi akwadebe ihe ndị mejupụtara simenti titanium gypsum nke nwere ezigbo arụmọrụ.
titaniumigwe igwe gypsum- HC Pendulum Raymond Mill
1. Gịnị ka itinye ihe dị iche iche na titanium gypsum nwere ike ime na arụmọrụ ya?
Ike nke titanium gypsum mgbe emezigharịrị anụ ahụ nwere oghere ụfọdụ na nke gypsum eke na gypsum kemịkalụ ndị ọzọ. A ga-etinye ụfọdụ ihe mgbakwunye iji melite ike nke titanium gypsum. Ihe mgbakwunye ejiri gụnyere ntụ desulfurization, ntụ ntụ, slag mmiri gwụchara, alum, ihe na-ebelata mmiri na ihe na-egbochi mmiri.
Mgbe ejiri slag emenyụ mmiri mee ihe dị ka ihe dị mfe, mgbe ọdịnaya ya erughị 40%, ọ gaghị emetụta ike nke ngwaahịa gypsum titanium, ọ nwekwara ike ibelata njupụta nke ngwaahịa ahụ nke ọma; Mgbe ọdịnaya nke ntụ ntụ erughị 30%, ọ na-enwe obere mmetụta n'imeziwanye ike nke titanium gypsum, mana mgbe ọdịnaya nke ntụ ntụ fly karịrị 30%, ọ ga-ebelata ike nke titanium gypsum, ntụ ntụ fly na-enyekwa aka imeziwanye ike ikpeazụ nke titanium gypsum (7d). Ash desulfured nwere ike imeziwanye ike nke titanium gypsum nke ukwuu. Site na mmụba nke ọdịnaya ya, ike nke ngwaahịa titanium gypsum nwere ike imeziwanye nke ukwuu. Alum nwere ike imeziwanye ike nke titanium gypsum nke ọma, mgbe ọdịnaya ya bụ 3%, mmetụta ya kacha mma; Oke mmiri agbakwunyere nwere mmetụta doro anya na ike nke titanium gypsum. Ka mmụba nke ọnụọgụ mmiri agbakwunyere, ike nke ihe nlele ahụ na-ebelata nke ukwuu. Ya mere, ebe ọ na-ahụ na mmiri nke pasta gypsum na-agbaze, obere mmiri agbakwunyere, ka mma.
Dịka ngwakọta dị mfe, slag a gbanyụrụ agbanyụ nwere ike ime ka njupụta nke ngwaahịa nnwale gypsum titanium dịkwuo mma. Ash a gbanyụrụ agbanyụ, ntụ ntụ a gbanyụrụ agbanyụ na alum nwere ike ime ka arụmọrụ ike nke gypsum titanium ka mma nke ukwuu. Ya mere, a na-ahọrọ gypsum titanium, ntụ a gbanyụrụ agbanyụ na ntụ ntụ a gbanyụrụ agbanyụ dị ka ntụ, a na-eji slag a gbanyụrụ agbanyụ dị ka ngwakọta dị mfe, a na-ejikwa alum, melamine na citric acid dị ka ihe mgbakwunye. A na-achọta paramita kachasị mma site na ịgbanwe oke nke ntụ. Oke nke mkpokọta bụ 40% nke ntụ, oke nke alum dị na mgbakwunye bụ 3% nke ntụ, oke nke melamine na citric acid bụ 1% n'otu n'otu, na mgbakwunye nke titanium gypsum 70% na ntụ a gbanyụrụ agbanyụ 30%, arụmọrụ nke ihe simenti dị mma.
2. Kedu otu esi akwadebe ihe mejupụtara simenti titanium gypsum nke nwere ezigbo arụmọrụ?
Mgbe a gbasasịrị ya ruo awa abụọ na okpomọkụ 600℃, a na-ejikọta gypsum titanium na ntụ ntụ, slag na simenti iji belata oge mmalite nke ihe mejupụtara ya ruo awa 3, oge ikpeazụ ịtọlite ruo awa 5, ike flexural 28d na ike nrụgide na-eru 4.3MPa na 13.6MPa n'otu n'otu. Site na titanium gypsum na slag dị ka ihe ndị bụ isi, enwere ike iji clinker simenti na ihe na-ebelata mmiri mbụ iji kwadebe simenti nwere arụmọrụ dị mma, ike ya na iguzogide mmiri doro anya karịa nke gypsum iwu ụlọ. Nnyocha ahụ na-egosi na ike nke ihe simenti agbakọtara na titanium gypsum mgbe emechara ọgwụgwọ eke ruo ụbọchị 28 nwere ike imezu ihe achọrọ maka ihe mgbidi ụlọ na ihe ndị agwakọtara agwakọta nke obodo, ọnụego mgbaze ya erughị 20% nke gypsum iwu ụlọ, ọnụego nnabata mmiri ya dịkwa ihe dị ka 50% nke gypsum iwu ụlọ, na-egosi na ihe simenti titanium gypsum mejupụtara ihe nwere ezigbo iguzogide mmiri. Ọ bụrụ na ihe simenti titanium gypsum fly ash slag agwakọtaghị ya na ihe na-eme ka ọ rụọ ọrụ, oge ntọala ya dị ogologo ma ike mbụ ya dị ala. Ịtinye simenti kwesịrị ekwesị na ihe simenti a nwere ike ime ka oge ntọala nke ihe simenti mejupụtara dị mkpụmkpụ, nke na-eme ka ike nke ihe simenti mejupụtara too.
Ụfọdụ nsonaazụ nyocha na-egosi na itinye simenti 5% na ihe mejupụtara simenti nke titanium gypsum fly ash slag nwere ike ime ka oge mmalite nke ihe mejupụtara simenti dị mkpụmkpụ ruo awa 4, oge ikpeazụ ịtọlite ruo awa 9, ike flexural 28d na ike nrụgide nwere ike iru 5.8MPa na 29.OMPa n'otu n'otu. Enwere ike ịkwadebe ihe mejupụtara simenti dị elu site na iji titanium gypsum, fly ash, slag na obere simenti Portland ma ọ bụ clinker, na-ahọrọ ihe na-eme ka ihe rụọ ọrụ kwesịrị ekwesị ma na-eme usoro kwesịrị ekwesị. Nnyocha ahụ na-egosi na itinye 5% alunite na ihe mejupụtara simenti nke titanium gypsum fly ash slag nwere ike ime ka oge mmalite nke ihe mejupụtara simenti dị mkpụmkpụ ruo awa 1, oge ikpeazụ ịtọlite ruo awa 2, na ike flexural 28d na ike nrụgide ruru 9.5 MPa na 53.0 MPa n'otu n'otu, na-eru ọkọlọtọ ike nke simenti 525R slag Portland.
3. Kedu ka ụdị ihe dị iche iche na-eme ka ihe rụọ ọrụ si emetụta ike nke ihe ndị mejupụtara simenti titanium gypsum?
Ike nke ihe mejupụtara simenti nwere ike ime ka ọ ka mma nke ukwuu mgbe ejiri gypsum titanium mee ka ọ ka mma. Ike nke ihe mejupụtara simenti nke simenti kpaliri naanị ya mụbara site na 70%, ike flexural na compressive nke ihe mejupụtara simenti mụbara ka ọdịnaya simenti mụbara. Mgbe ọdịnaya simenti dị 15%, ike ya kacha elu. Mgbe ọdịnaya lime dị 15%, ọdịnaya simenti bụ 0, ike ya dịkwa ala. Na sistemụ gypsum fly ash nke titanium, iji ihe mkpali simenti na-eme ka ike nke sistemụ dịkwuo mma.
Ọ bụrụ na ịchọrọtitaniumigwe igwe gypsum, please contact mkt@hcmilling.com or call at +86-773-3568321, HCM will tailor for you the most suitable grinding mill program based on your needs, more details please check www.hcmilling.com.Onye injinia anyị ga-eme atụmatụ maka nhazi akụrụngwa sayensị maka gị ma tụọ aro maka gị.
Oge ozi: Disemba-05-2022